Influence of temperature on threshold stress for reorientation of hydrides and residual stress variation across thickness of Zr-2.5Nb alloy pressure tube

Singh, R.N. ; Lala Mikin, R. ; Dey, G.K. ; Sah, D.N. ; Batra, I.S. and Ståhle, Per LU (2006) In Journal of Nuclear Materials 359(3). p.208-249
Abstract
Threshold stress, σth, for reorientation of hydrides in cold worked and stress-relieved (CWSR) Zr–2.5Nb pressure tube material was determined in the temperature range of 523–673 K. Using tapered gage tensile specimen, mean value of σth was experimentally determined by two methods, half thickness method and area compensation method. The difference between local values of σth measured across the thickness of the tube and the mean σth values yielded the residual stress variation across the tube thickness. It was observed that both the mean threshold stress and residual stress decrease with increase in reorientation temperature. Also, the maximum value of residual stresses was observed near the midsection of the tube.
Please use this url to cite or link to this publication:
author
; ; ; ; and
organization
publishing date
type
Contribution to journal
publication status
published
subject
in
Journal of Nuclear Materials
volume
359
issue
3
pages
208 - 249
publisher
Elsevier
external identifiers
  • scopus:33751218602
ISSN
0022-3115
DOI
10.1016/j.jnucmat.2006.09.004
language
English
LU publication?
yes
id
12bc0d64-1ab1-4233-943f-b2206cb65dd7 (old id 960695)
date added to LUP
2016-04-01 12:13:11
date last changed
2022-03-28 21:51:25
@article{12bc0d64-1ab1-4233-943f-b2206cb65dd7,
  abstract     = {{Threshold stress, σth, for reorientation of hydrides in cold worked and stress-relieved (CWSR) Zr–2.5Nb pressure tube material was determined in the temperature range of 523–673 K. Using tapered gage tensile specimen, mean value of σth was experimentally determined by two methods, half thickness method and area compensation method. The difference between local values of σth measured across the thickness of the tube and the mean σth values yielded the residual stress variation across the tube thickness. It was observed that both the mean threshold stress and residual stress decrease with increase in reorientation temperature. Also, the maximum value of residual stresses was observed near the midsection of the tube.}},
  author       = {{Singh, R.N. and Lala Mikin, R. and Dey, G.K. and Sah, D.N. and Batra, I.S. and Ståhle, Per}},
  issn         = {{0022-3115}},
  language     = {{eng}},
  number       = {{3}},
  pages        = {{208--249}},
  publisher    = {{Elsevier}},
  series       = {{Journal of Nuclear Materials}},
  title        = {{Influence of temperature on threshold stress for reorientation of hydrides and residual stress variation across thickness of Zr-2.5Nb alloy pressure tube}},
  url          = {{http://dx.doi.org/10.1016/j.jnucmat.2006.09.004}},
  doi          = {{10.1016/j.jnucmat.2006.09.004}},
  volume       = {{359}},
  year         = {{2006}},
}