Refinement of microstructure and mechanical properties of titanium processed by twist extrusion and subsequent rolling

Stolyarov, V. V.; Beigel'zimer, Ya E.; Orlov, D. V. LU and Valiev, R. Z. (2005) In Physics of Metals and Metallography 99(2). p.204-211
Abstract

Microstructure and mechanical properties as well as thermal stability of commercially pure titanium VT1-0 subjected to severe plastic deformation by twist extrusion (TE) were studied before and after low-temperature annealing and cold rolling. TE leads to a refinement of structural fragments to sizes of less than 1 μm, enhancement of strength, and the appearance of strong anisotropy of mechanical properties. Subsequent low-temperature annealing increases plasticity of the deformed titanium, retaining its enhanced strength. A combined treatment (TE and rolling) results in an additional refinement of the microstructure, which remains thermally stable to 300-350°C, and changes the anisotropy of mechanical properties.

Please use this url to cite or link to this publication:
author
publishing date
type
Contribution to journal
publication status
published
subject
in
Physics of Metals and Metallography
volume
99
issue
2
pages
8 pages
publisher
Maik Nauka-Interperiodica Publishing
external identifiers
  • scopus:17144390666
ISSN
0031-918X
language
English
LU publication?
no
id
53038f8e-c3cd-454a-995f-8ed8e1d03756
date added to LUP
2016-06-20 15:45:14
date last changed
2017-09-10 05:07:11
@article{53038f8e-c3cd-454a-995f-8ed8e1d03756,
  abstract     = {<p>Microstructure and mechanical properties as well as thermal stability of commercially pure titanium VT1-0 subjected to severe plastic deformation by twist extrusion (TE) were studied before and after low-temperature annealing and cold rolling. TE leads to a refinement of structural fragments to sizes of less than 1 μm, enhancement of strength, and the appearance of strong anisotropy of mechanical properties. Subsequent low-temperature annealing increases plasticity of the deformed titanium, retaining its enhanced strength. A combined treatment (TE and rolling) results in an additional refinement of the microstructure, which remains thermally stable to 300-350°C, and changes the anisotropy of mechanical properties.</p>},
  author       = {Stolyarov, V. V. and Beigel'zimer, Ya E. and Orlov, D. V. and Valiev, R. Z.},
  issn         = {0031-918X},
  language     = {eng},
  number       = {2},
  pages        = {204--211},
  publisher    = {Maik Nauka-Interperiodica Publishing},
  series       = {Physics of Metals and Metallography},
  title        = {Refinement of microstructure and mechanical properties of titanium processed by twist extrusion and subsequent rolling},
  volume       = {99},
  year         = {2005},
}