Composition-Dependent Alloy Nanoparticle Shape Changes under Reaction Conditions : Kinetic and Thermodynamic Effects

Hejral, U. LU ; Plessow, P. N. ; Franz, D. ; Shipilin, M. LU ; Gutowski, O. ; Rütt, U. ; Noei, H. ; Vonk, V. and Stierle, A. (2024) In Journal of Physical Chemistry C 128(10). p.4330-4342
Abstract

Particle sintering and reshaping constitute the main cause for catalyst deactivation. An atomic-scale understanding of the correlation among the catalyst structure, its support, and the gas phase under realistic reaction conditions is required for its suppression. In this study, we combined high-energy grazing incidence X-ray diffraction, in situ mass spectrometry, ex situ scanning electron microscopy, and density functional theory calculations to unravel the driving force behind the composition-dependent particle shape changes and sintering processes of α-Al2O3(0001)-supported Pt-Pd alloy nanoparticles under realistic reaction conditions for CO oxidation. We find that pure Pt and Pt-rich particles, initially... (More)

Particle sintering and reshaping constitute the main cause for catalyst deactivation. An atomic-scale understanding of the correlation among the catalyst structure, its support, and the gas phase under realistic reaction conditions is required for its suppression. In this study, we combined high-energy grazing incidence X-ray diffraction, in situ mass spectrometry, ex situ scanning electron microscopy, and density functional theory calculations to unravel the driving force behind the composition-dependent particle shape changes and sintering processes of α-Al2O3(0001)-supported Pt-Pd alloy nanoparticles under realistic reaction conditions for CO oxidation. We find that pure Pt and Pt-rich particles, initially kinetically trapped in metastable flat particle shapes, undergo a strong reaction-induced height increase to adopt a more stable, theoretically predicted compact equilibrium shape. Contrarily, Pd-rich particles prove to be more resistant against shape changes, since they exhibit already a shape close to equilibrium. We thus conclude that the observed initial deviations in particle shape from the theoretical predictions are due to kinetic limitations during growth. Our data provide information on the segregation state of the alloy particles, indicating a Pt core and Pd shell structure under strongly reducing conditions and the alloying of Pt and Pd under the reaction conditions for CO oxidation close to stoichiometry.

(Less)
Please use this url to cite or link to this publication:
author
; ; ; ; ; ; ; and
organization
publishing date
type
Contribution to journal
publication status
published
subject
in
Journal of Physical Chemistry C
volume
128
issue
10
pages
13 pages
publisher
The American Chemical Society (ACS)
external identifiers
  • scopus:85186416519
ISSN
1932-7447
DOI
10.1021/acs.jpcc.4c00042
language
English
LU publication?
yes
id
f375633c-656b-45e9-b380-b67cd0700d2e
date added to LUP
2024-03-27 10:36:55
date last changed
2024-03-27 10:37:56
@article{f375633c-656b-45e9-b380-b67cd0700d2e,
  abstract     = {{<p>Particle sintering and reshaping constitute the main cause for catalyst deactivation. An atomic-scale understanding of the correlation among the catalyst structure, its support, and the gas phase under realistic reaction conditions is required for its suppression. In this study, we combined high-energy grazing incidence X-ray diffraction, in situ mass spectrometry, ex situ scanning electron microscopy, and density functional theory calculations to unravel the driving force behind the composition-dependent particle shape changes and sintering processes of α-Al<sub>2</sub>O<sub>3</sub>(0001)-supported Pt-Pd alloy nanoparticles under realistic reaction conditions for CO oxidation. We find that pure Pt and Pt-rich particles, initially kinetically trapped in metastable flat particle shapes, undergo a strong reaction-induced height increase to adopt a more stable, theoretically predicted compact equilibrium shape. Contrarily, Pd-rich particles prove to be more resistant against shape changes, since they exhibit already a shape close to equilibrium. We thus conclude that the observed initial deviations in particle shape from the theoretical predictions are due to kinetic limitations during growth. Our data provide information on the segregation state of the alloy particles, indicating a Pt core and Pd shell structure under strongly reducing conditions and the alloying of Pt and Pd under the reaction conditions for CO oxidation close to stoichiometry.</p>}},
  author       = {{Hejral, U. and Plessow, P. N. and Franz, D. and Shipilin, M. and Gutowski, O. and Rütt, U. and Noei, H. and Vonk, V. and Stierle, A.}},
  issn         = {{1932-7447}},
  language     = {{eng}},
  number       = {{10}},
  pages        = {{4330--4342}},
  publisher    = {{The American Chemical Society (ACS)}},
  series       = {{Journal of Physical Chemistry C}},
  title        = {{Composition-Dependent Alloy Nanoparticle Shape Changes under Reaction Conditions : Kinetic and Thermodynamic Effects}},
  url          = {{http://dx.doi.org/10.1021/acs.jpcc.4c00042}},
  doi          = {{10.1021/acs.jpcc.4c00042}},
  volume       = {{128}},
  year         = {{2024}},
}